Analysis of Variation in the Number of Layers in the Hardfacing Process of ASTM A216 WCB Material on Hardness, Wear, and Microstructure
10 Halaman
Penulis
ISSN
2623-2197
Penerbit
Universitas Andi Djemma Palopo
Diterbitkan pada
08/11/2025
Bahasa
English
Kata Kunci
Abstrak
ASTM A216 WCB material is a cast carbon steel commonly used in valve components operating at high temperatures, where one of the main problems is surface wear. This study aims to analyze the effect of variations in the number of Stellite 12 hardfacing layers and the type of buffer layer (ER308 and ER309) on the hardness, wear resistance, and microstructure of ASTM A216 WCB material. Four variations of specimens were tested using the Gas Tungsten Arc Welding (GTAW) welding process. The hardness test results showed that increasing the number of layers consistently increased the material hardness due to reduced dilution and microstructural refinement. The highest hardness value of 477.89 HV was recorded in the specimen with the ER309 buffer layer and four layers of hardfacing. In contrast, the lowest wear rate, which indicates the highest wear resistance, was 0.00318 mm³/Nm and was observed in the specimen with the ER308 buffer layer and two layers of hardfacing, which had a lower surface hardness (396.13 HV). These results indicate a non-linear relationship between maximum hardness and optimal wear performance. Microstructural observations indicate that the base metal has a ferrite and pearlite structure. In the buffer layer, austenite and vermicular ferrite structures are formed. Meanwhile, in the hardfacing layer, α-dendritic phases and complex carbide precipitation were found, which were presumptively identified as M23C6. This study concludes that optimizing hardfacing performance on WCB steel requires a balance between the hardness achieved through the number of layers and the microstructural toughness influenced by the interaction with the buffer layer.