The radiopacity of glass ionomer cement after addition of nHA powder: experimental study
7 Halaman
Penulis
ISSN
2549-6514 (ONLINE)
Penerbit
Fakultas Kedokteran Gigi Universitas Padjadjaran, Indonesia
Diterbitkan pada
31/08/2023
Bahasa
English
Kata Kunci
Abstrak
Introduction: One of the restorative materials often used in dental restoration treatment is GIC. One type of GIC is conventional GIC. Conventional GIC has the disadvantage of having low compressive strength compared to resin-modified GIC and high viscosity. One of the efforts to improve the mechanical properties of GIC is by adding nano hydroxyapatite (nHA) which can be obtained from natural materials such as eggshells. The addition of nHA to GIC can increase the compressive strength of GIC and the addition of nHA is thought to result in a change in the radiopacity properties of GIC. The research aims to analyze the radiopacity of GIC after the addition of nano-hydroxyapatite powder. Methods: The number of samples was 24 discs with a diameter of 7 mm and a height of 3 mm which were divided into 4 group. The research group was K0 (GIC) as the control group, K1 (GIC+ 2% nHA), K2 (GIC+ 3% nHA), and K3 (GIC + 4% nHA). Radiopacity measurements were carried out using the J Image application. Results: The results of the ANOVA test was p<0.05, which means that the radiopacity values in each group had a significant difference. The average gray value of GIC without the addition of nHA (K0) was 206.5, GIC + 2% nHA (K1) was 233.0, GIC + 3% nHA (K2) was 237.8 and GIC + 4% nHA (K3) was 241.0 measured with Image J. Conclusions: The addition of nHA powder can increase the radiopacity of GIC and 4% nHA powder added to GIC has the highest radiopacity value compared to 2 and 3% nHA powder added to GIC. .